Serious question, I ran my roughing passes dry on 4140 steel and the finish came out better
Everyone at my shop in Dayton says you gotta flood coolant on 4140 or you'll cook the inserts, so I tried dry roughing on a batch of 30 parts just to see. The inserts lasted 40 minutes longer per edge and the chips came off like glass instead of that nasty birds nest. I ran 550 SFM with a 0.012 feed and the spindle load stayed lower the entire time. My lead man said I was nuts, but the numbers on the tool log don't lie. Has anyone else had dry roughing beat coolant on medium carbon steel, or did I just get lucky with this heat lot?