Just realized coolant nozzles aren't meant to spray right at the flute tip
A guy on the night shift at our plant in Rockford pointed out that I had my coolant aimed dead at the tip of the end mill, which is why I kept getting chip weld on 6061 after about 40 minutes of run time. He moved the nozzle back to flood the whole pocket and my tool life jumped from around 3 hours to almost 9 per insert on the same job. Has anyone else been aiming coolant at the cut instead of just drowning the whole area?